Copper metallurgy equipment

The blast furnace is one of the most important metallurgical equipment,it has the following characteristics:high thermal efficiency,high specific productivity(specific capacity),high metal recovery rate,low cost,less covering area and so on.

Copper metallurgy equipment

Sintering machine

 Sintering machine is suitable for sintering operation of large ferrous metallurgy sintering factory,which is the main equipment in exhaust sintering process.It can sinter different components,different particle concentrate powder and rich-mineral powder to blocks,and partly eliminate sulfur harmful substance(such as sulfur,phosphorus etc.)in ore.The larger the sintering area,the more the yield.

Sintering machine

secondary lead metallurgy equipment

It is good to use converter to dispose lead-acid battery plate for secondary lead.Converter has higher thermal efficiency,higher operation rate than reverberatory furnace,it also has some advantages as below:high degree of mechanization,good working conditions,good environment protection effect.

secondary lead metallurgy equipment

zinc oxide metallurgy equipment

The rotary kiln has high production capacity,high degree of mechanization,simple operation and maintenance,can adapt to a variety of industrial raw materials sintering,roasting,evaporation,calcination,segregation and other processes.It is widely used in metallurgy industry,cement industry,refractories industry,chemical industry etc..

zinc oxide metallurgy equipment

The main technical conditions of lead smelting in blast furnace

2014-08-12 15:37:02

The input quantity 

    Each input quantity of blast furnace depends on the furnace size,large furnace can reach 1~3.5t ,small furnace just can reach 100~500kg.Feeding time interval usually be 10 ~ 20 min, material surface wave can not more than 0.5 m before and after feeding. 

The stock column height 

    Lead blast furnace has two operation methods-- with high stock column (3.6 ~ 6.0 m) and with low stock column (2.5 ~ 3 m), generally we use the former one. When any of the following special circumstances, we can consider to use low stock column operation: (1) sintering block has higher lead grade (more than 50%), high residual S;(2) low sintering block strength;(3) to obtain a higher hearth efficiency 80~90t/(m2•d-1);(4) small blast furnace smelting.

Blast volume and air pressure 

    In production, when we use high stock column operation,blast strength is 25 ~ 35 m3•m-2•min-1; when we use low stock column operation,blast strength is 40 ~ 60 m3•m-2•min-1.The blast pressure of blast furnace mainly depends on the resistance of stock column in furnace, and fluctuates according to the furnace condition. When high stock column operations, generally it is about 11 ~ 20 kpa;when low stock column operations, generally it is about 6.7 ~ 11 kpa.When the blast furnace has a larger tuyere zone width or small outlet, we should take higher blast pressure, conversely take lower blast pressure. 

Liquid lead, slag discharge temperature and furnace top pressure 

    Lead liquid discharge temperature is 800 ~ 1000 ℃, slag temperature is 1100 ~ 1200 ℃.In order to prevent roof smoke and a lot of air leakage, we should control the negative pressure operation, top pressure is commonly l0 ~ 50 pa. 

Coke rate 

    When we take high stock column operations, we control coke rate to be general 10% ~ 13%;When low stock column,we control coke rate to be 7.50 ~ 10%. 

Blast furnace water jacket supply water 

    Water jacket cooling way has two kinds-- water cooling and evaporative cooling.When we take water cooling, for water supply,it has the following requirements: 

(1) the general water temperature at the outlet is 60 ~ 80 ℃, take lower limit when the water hardness is bigger, conversely take the ceiling;

(2) when the water temperature difference between import and export is 40 ~ 60 ℃, the water consumption of unit water jacket area is 16 l/m2 (min), also can estimate according to 2~4m3 water consumption per ton burden. 

Be controled by lead liquid surface and slag surface in furnace hearth 

    When the blast pressure is 13.3 ~ 17.3 kPa,the lead liquid level of siphon lead well generally higher than the lead level in furnace hearth in 100 ~ 250 mm. The lead level in well is controlled by mud weir of lead chute. If the lead liquid level is too high, partial lead will be taken out through the discharge of slag and matte;If it is too low, matte can not discharge in time, it is easy to form furnace accretion. When the blast pressure is 11-17.3 kPa, throat bottom below the siphon well lead level 50 ~ 100 mm;the throat mouth slag dam height is generally 350 ~ 450 mm. 